TECAPEEK® CM XP109 COMPUESTO DE PEEK NEGRO
Obtener el último precioTipo de Pago: | T/T,Paypal |
Cantidad de pedido mínima: | 1 Kilogram |
transporte: | Ocean,Land,Air,Express |
Hafen: | Shenzhen,Guangzhou,Hongkong |
Tipo de Pago: | T/T,Paypal |
Cantidad de pedido mínima: | 1 Kilogram |
transporte: | Ocean,Land,Air,Express |
Hafen: | Shenzhen,Guangzhou,Hongkong |
Modelo: TECAPEEK® CM XP109 BLACK PEEK
Marca: Tecapeek
Unidades de venta | : | Kilogram |
Tipo de paquete | : | Paquete de exportación |
The file is encrypted. Please fill in the following information to continue accessing it
Tecapeek CM XP109 Black Peek Mod. 30% de fibra de carbono y 15% PTFE
Este material moldeado por compresión es un polímero Victrex® Peek modificado con fibra de carbono al 30% y al 15% de PTFE para mejorar las propiedades de deslizamiento y desgaste, y una mayor resistencia.
HECHOS
Designación química
PIEK (polietheretherketona)
Color
negro
Densidad
1.51 g/cm3
PRINCIPALES CARACTERÍSTICAS
Retardante de la llama inherente
Buena temperatura de deflexión de calor
hidrólisis y resistente a vapor sobrecalentado
buena maquinabilidad
Buenas propiedades de deslizamiento y desgaste
Industrias objetivo
Industria de petróleo y gas
PEEK Compound: 30% carbon fiber with 15% PTFE | ||||
Properties | ASTM | Units | Typical Values | |
Test Method | ||||
Mechanical | Tensile Strength | D-638 | psi | 11,800 |
Tensile Elongation | D-638 | % @ Yield | 1.3 | |
Tensile Elongation | D-638 | % @ Break | 1.8 | |
Tensile Modulus | D-638 | psi | 1,520,000 | |
Flexural Strength | D-790 | psi | 15,500 | |
Flexural Modulus | D-790 | psi | 1,500,000 | |
Flexural Strain | D-790 | % | - | |
Compressive Strength (1%) | D-695 | psi | 7,700 | |
Compressive Strength (10%) | D-695 | psi | 20,500 | |
Compressive Modulus | D-695 | psi | 720,000 | |
Izod Impact Strength (Notched) | D-256 | ft-lb/in | 0.68 | |
Shear Strength | D-732 | psi | - | |
Hardness | D-2240 | Shore D | 90 | |
Hardness | D-785 | Rockwell (M) | - | |
Thermal | Heat Distortion Temperature | D-648 | ℉ | - |
Coefficient of Linear | E-831 | 10-6/℉ | - | |
Thermal Expansion | ||||
Thermal Conductivity | C-177 | BTU in/hr-ft2-℉ | - | |
Continuous Use (Mechanical) | UL746B | 。 | - | |
Limiting Oxygen Index | D-2863 | %O2 | - | |
Melt Point | DSC | ℉ | 649 | |
Electrical | Dielectric Strength | D-149 | KVcm | - |
Dielectric Constant | D-150 | 50Hz, 200℃ | - | |
Volume Resistivity | D-257 | ohm-cm | - | |
Surface Resistivity | D-257 | ohm/sq | - | |
Physical | Specific Gravity | D-792 | gm/cm3 | 1.51 |
Color | - | - | Black | |
Filler Content | - | % | 45 | |
Water Absorption (RT 24h) | D-570 | % | - | |
Typical Level of Crystallinity | - | % | - | |
Other | Static Coefficient of Friction | D-1894 | - | - |
Kinetic Coefficient of Friction | D-1894 | - | - |
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.